EU RO PEAN COMMISSION SCIENCE RESEARCH DEVELOPMENT technical steel research Measurement and analysis Surface analysis of non-conductive coatings by radio frequency glow discharge optical emission spectrometry hi Report EUR 18468 EN STEEL RESEARCH EUROPEAN COMMISSION Edith CRESSON, Member of the Commission responsible for research, innovation, education, training and youth DG XII/C.2 — RTD actions: Industrial and materials technologies — Materials and steel Contact: Mr H. J.-L. Martin Address: European Commission, rue de la Loi 200 (MO 75 1/10), B-1049 Brussels — Tel. (32-2) 29-53453; fax (32-2) 29-65987 European Commission E tø if w1 %f * Measurement and analysis Surface analysis of non-conductive coatings by radio frequency glow discharge optical emission spectrometry N. Zacchetti, M. Cilia, M. Del Monte, E. Lo Piccolo Centro Sviluppo Materiali SpA Via di Castel Romano 100-102 1-00129 Rome Contract No 7210-GD/410 1 July 1992 to 31 December 1995 Final report Directorate-General Science, Research and Development 1998 EUR 18468 EN LEGAL NOTICE Neither the European Commission nor any person acting on behalf of the Commission is responsible for the use which might be made of the following information. A great deal of additional information on the European Union is available on the Internet. It can be accessed through the Europa server (http://europa.eu.int). Cataloguing data can be found at the end of this publication.